Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 10.9 g/m²/day @Thickness 0.0254 mm |
0.702 g/100 in²/day @Thickness 0.00100 in |
2.5 BUR; ASTM F1249 |
Total HL 428 HDPE Film Grade Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro.. |