Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 6.05 g/m²/day @Temperature 38.0 °C |
0.390 g/100 in²/day @Temperature 100 °F |
90% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 35MW647 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performances on all types of packaging machines.Availability: Africa & .. |
|||
Water Vapor Transmission | 6.05 g/m²/day @Temperature 38.0 °C |
0.390 g/100 in²/day @Temperature 100 °F |
90% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 33MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |