Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 3.41 g/m²/day @Temperature 38.0 °C |
0.220 g/100 in²/day @Temperature 100 °F |
90% RH; ExxonMobil Method |
ExxonMobil Oppalyte™ 50MO747 OPP Film Product Description: A white opaque biaxially oriented polypropylene film, coated on one side acrylic, one side PVdC. Provides excellent performance on all packaging machines.Availability: Africa & .. |