Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 1.20 g/m²/day @Temperature 38.0 °C |
0.0770 g/100 in²/day @Temperature 100 °F |
90% RH; ExxonMobil Method |
ExxonMobil Metallyte™ 30MM680 OPP Film Product Description: A biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. Typically, all gauges are used laminated with other substrates on HFFS and VFFS .. |