Polymer Property : Saybolt Viscosity at 210°F = 89 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 89 SUS
89 SUS
ChevronTexaco Drive Train Fluid HD, SAE 50
FeaturesChevron Drive Train Fluids HD are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 ..
Saybolt Viscosity at 210°F 89 SUS
89 SUS
ChevronTexaco SAE 50 Transmission and Drive Train TO-4 Oil
Texaco Transmission and Drive Train TO-4 Oils deliver value through:Longer equipment life — Special additives protect metal surfaces against scuffing and wear even under severe operating conditions..
Saybolt Viscosity at 210°F 89 SUS
89 SUS
ConocoPhillips Hydroclear® MV150 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..