Polymer Property : Saybolt Viscosity at 210°F = 79 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 79 SUS
79 SUS
ConocoPhillips El Mar® Grade 15W-40 Geo Oil
Description: Conoco El Mar® Geo Oil is a high-quality, rust- and oxidation-inhibited, nondetergent, ashless gas engine oil. It is formulated with high viscosity index paraffinic base oils blended w..
Saybolt Viscosity at 210°F 79 SUS
79 SUS
ConocoPhillips Hydroclear® 150 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Saybolt Viscosity at 210°F 79 SUS
79 SUS
ConocoPhillips 150 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Saybolt Viscosity at 210°F 79 SUS
79 SUS
ConocoPhillips 150 Gear Oil AGMA Lubricant No. 4 EP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..