Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 78.1 SUS | 78.1 SUS | |
ChevronTexaco 150 PMO ashless Texaco PMO Ashless oils deliver value through:High temperature stability — Contain an effective oxidation inhibitor to protect the oil at elevated ambient operating temperatures.Long lubricant life.. |
|||
Saybolt Viscosity at 210°F | 78.1 SUS | 78.1 SUS | |
ChevronTexaco Clarity® ISO 150 Paper Machine Oil FeaturesChevron Clarity Paper Machine Oils are the next generation circulating oils for the pulp and paper industry.Chevron Clarity Paper Machine Oils ISO 100, 150, and 220 are formulated with ISOS.. |