Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 75.8 SUS | 75.8 SUS | |
ChevronTexaco Rykon® ISO 100 Premium Oil FeaturesChevron Rykon Premium Oils are designed to give maximum protection to hydraulic pumps.They are formulated with ISOSYN® base stocks incorporating antiwear additives, oxidation and corrosion .. |