Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 75.6 SUS | 75.6 SUS | |
ChevronTexaco Rando® HDZ 100 Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor.. |