Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 73.8 SUS | 73.8 SUS | |
ChevronTexaco HiPerSYN™ ISO 100 Oil FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation
stability, high viscosity index, high flash point, low pour point, and e.. |