Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 72 SUS | 72 SUS | |
ExxonMobil Teresstic 150 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Saybolt Viscosity at 210°F | 72 SUS | 72 SUS | |
ConocoPhillips SynXPA® 150 R&O Oil Description: Conoco SynXPA R&O Oil lubricates stationary and portable rotary compressors, as well as reciprocating compressors that operate in severe service. It is useful in single- and double-acti.. |
|||
Saybolt Viscosity at 210°F | 72 SUS | 72 SUS | |
ChevronTexaco Capella® HFC Auto Texaco Capella HFC Auto delivers value through:Long service life and cleaner systems — Provides chemical and thermal stability.High miscibility with R-134a — Allows ready lubricant flow in low tem.. |
|||
Saybolt Viscosity at 210°F | 72 SUS | 72 SUS | |
ExxonMobil Teresstic 150 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Saybolt Viscosity at 210°F | 72 SUS | 72 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® FGC 40 Compressor Fluid, Synthetic Food Grade ISO 100 Description: ANDEROL FGC 40 Compressor Fluid is a synthetic hydrocarbon (PAO) based lubricant formulated for use in compressors. FGC 40 Fluid meets the former H-1 approval requirements of the USDA w.. |
|||
Saybolt Viscosity at 210°F | 72 SUS | 72 SUS | |
ConocoPhillips El Mar® Grade 30-40 Geo Oil Description: Conoco El Mar® Geo Oil is a high-quality, rust- and oxidation-inhibited, nondetergent, ashless gas engine oil. It is formulated with high viscosity index paraffinic base oils blended w.. |
|||
Saybolt Viscosity at 210°F | 72 SUS | 72 SUS | |
ChevronTexaco Black Pearl® NLGI 0 Grease EP FeaturesChevron Black Pearl Greases EP are multipurpose, extreme pressure, water-resistant greases.They are formulated with ISOSYN® base stock, a polyurea thickener, and rust and oxidation inhibito.. |
|||
Saybolt Viscosity at 210°F | 72 SUS | 72 SUS | |
ChevronTexaco Black Pearl® NLGI 1 Grease EP FeaturesChevron Black Pearl Greases EP are multipurpose, extreme pressure, water-resistant greases.They are formulated with ISOSYN® base stock, a polyurea thickener, and rust and oxidation inhibito.. |
|||
Saybolt Viscosity at 210°F | 72 SUS | 72 SUS | |
ChevronTexaco Snow White Petrolatum, Snow White Chevron Petrolatums are ash-free mixtures of mineral oils and a special petroleum wax with a smooth grease-like texture.ApplicationsChevron Petrolatums find wide use in pharmasutical and cosmetic pr.. |