Polymer Property : Saybolt Viscosity at 210°F = 71 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 71 SUS
71 SUS
See Note 3.
ChevronTexaco PremiumRB
Texaco Premium RB delivers value through:Wide application range — Suitable for high rpm operation, operating temperatures ranging from -34°C to 177°C (-30°F to 350°F) and offers excellent rust ..