Polymer Property : Saybolt Viscosity at 210°F = 584 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 584 SUS
584 SUS
ChevronTexaco Sugartex®
Texaco Sugartex delivers value through:Reliability — High lubricant film strength withstands heavy shock loads and provides protection under boundary lubrication to minimize wear rate and prevent f..