Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 56.7 SUS
56.7 SUS
ChevronTexaco ISO 100 Saw Guide Oil
FeaturesChevron Saw Guide Oil is manufactured using naphthenic oils and specially selected additives balanced to reduce friction between saw and guide components in thin kerf saw equipment. These ad..