Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 52 SUS | 52 SUS | |
ChevronTexaco ParaMount™ 3005 Paraffinic Process Oil FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur.. |
|||
Saybolt Viscosity at 210°F | 52 SUS | 52 SUS | |
ChevronTexaco Transultex® H Texaco Transultex metalworking fluids deliver value through:Excellent antiweld properties from active sulfur and chlorine which reduce frictional heat, prevent welding of metal to the tool point, ex.. |
|||
Saybolt Viscosity at 210°F | 52 SUS | 52 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® FGC 20 Synthetic Food Grade Compressor Fluid, ISO 46 Description: ANDEROL FGC Series Compressor Fluids are synthetic hydrocarbon (PAO) based lubricants formulated for use in compressors. FGC Series Fluids meet the former H-1 approval requirements of t.. |
|||
Saybolt Viscosity at 210°F | 52 SUS | 52 SUS | |
ChevronTexaco Bright-Cut® AXH Metal Working Fluid FeaturesChevron Bright-Cut Metalworking Fluids are a complete line of chlorine-free cutting oils that offer benefits not found in conventional cutting oils.The unique synthetic antiweld components .. |
|||
Saybolt Viscosity at 210°F | 52 SUS | 52 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® FGH 46 Synthetic Food Grade Hydraulic Fluid, ISO 46 Description: ANDEROL FGH Series Hydraulic Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA wh.. |