Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 48.4 SUS
48.4 SUS
ChevronTexaco Canopus® 46
Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant ..
Copyright © lookpolymers.com All Rights Reserved