Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 47.4 SUS
47.4 SUS
ChevronTexaco 46 Heat Transfer Oil
FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont..
Saybolt Viscosity at 210°F 47.4 SUS
47.4 SUS
ChevronTexaco Rykon® ISO 32 Premium Oil
FeaturesChevron Rykon Premium Oils are designed to give maximum protection to hydraulic pumps.They are formulated with ISOSYN® base stocks incorporating antiwear additives, oxidation and corrosion ..
Saybolt Viscosity at 210°F 47.4 SUS
47.4 SUS
ChevronTexaco Texatherm®
Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging ..