Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 45.7 SUS | 45.7 SUS | |
ChevronTexaco Vistac® ISO 32 Way Oil D FeaturesChevron Way Oils Vistac D are high quality lubricants designed to meet the critical lubrication demands for the slides and ways of machine tools.Chevron Way Oils Vistac D is formulated with .. |
|||
Saybolt Viscosity at 210°F | 45.7 SUS | 45.7 SUS | |
ChevronTexaco WAY 32 Hydraulic Texaco Hydraulic-Way 32 delivers value through:Excellent separation from metalworking coolants — The SKC (SKC Gleittechnik) coolant separation test showed excellent separation from a wide variety o.. |
|||
Saybolt Viscosity at 210°F | 45.7 SUS | 45.7 SUS | |
ChevronTexaco Pinnacle® 32 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |