Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 42 SUS | 42 SUS | |
ExxonMobil Vacmul 3 A Vacmul 3 A is a non-staining, low-viscosity mineral oil, intended for use as an EDM fluid or as a light- to moderate-duty honing oil. |
|||
Saybolt Viscosity at 210°F | 42 SUS | 42 SUS | |
ConocoPhillips Syncon® 22 Synthetic AW Hydraulic Fluid 22 Syncon AW Hydraulic Fluid is a premium quality, synthetic antiwear hydraulic fluid developed for use in industrial and mobile equipment operating at extreme temperatures. It is particularly recommen.. |
|||
Saybolt Viscosity at 210°F | 42 SUS | 42 SUS | |
ChevronTexaco Quenchtex® B Texaco Quenchtex oils deliver value through:Controlled cooling of metals — Combines the high initial quenching speed of water with slow final quenching speed of oil.Safety — High flash point and f.. |
|||
Saybolt Viscosity at 210°F | 42 SUS | 42 SUS | |
ChevronTexaco Vistac® ISO 32 Rock Drill Oil FeaturesChevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.They are formulated from highly refined, high viscosity index, paraffinic base stocks and add.. |
|||
Saybolt Viscosity at 210°F | 42 SUS | 42 SUS | |
ExxonMobil Vacmul 3 A Vacmul 3 A is a non-staining, low-viscosity mineral oil, intended for use as an EDM fluid or as a light- to moderate-duty honing oil. |
|||
Saybolt Viscosity at 210°F | 42 SUS | 42 SUS | |
ConocoPhillips 32 Spectrum Cutting Oil Description: Conoco Spectrum Cutting Oil is a multifunctional cutting fluid formulated with a sulfurized base oil, is a balanced additive system and is suited for a wide variety of machining applica.. |
|||
Saybolt Viscosity at 210°F | 42 SUS | 42 SUS | |
ChevronTexaco Trough Grease Soft Chevron Trough Grease Soft is a soft petrolatum formulation used to grease the sides of troughs in which dough is allowed to rise, which prevents the dough from adhering to the sides.ApplicationsChe.. |