Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 41.3 SUS | 41.3 SUS | |
ChevronTexaco 22 Heat Transfer Oil FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont.. |