Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 39.8 SUS
39.8 SUS
ChevronTexaco ISO 22 CP Oil
FeaturesChevron CP Oil is used for both cotton picker spindle lubrication and as a corrosion (rust) preventative on steel materials in the steel industry.It is manufactured form medium viscosity ind..