Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 37.1 SUS | 37.1 SUS | |
ChevronTexaco ISO 15 Handy Oil FeaturesChevron Handy Oil is a highly refined, light-bodied, multipurpose lubricating oil.It contains an oxidation inhibitor to improve its natural stability and prevent the formation of gums and va.. |