Polymer Property : Saybolt Viscosity at 210°F = 34 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 34 SUS
34 SUS
ChevronTexaco Almag® Oil
Texaco Almag oil delivers value through:Low viscosity that provides faster wetting of metal surfaces and penetration to the cutting zone.Excellent cooling properties, carrying heat away from the cut..
Saybolt Viscosity at 210°F 34 SUS
34 SUS
ChevronTexaco Concrete Form Oil VOC
Texaco Concrete Form Oil VOC delivers value through:Clean separation from forms — imparts an excellent surface finish to concrete.Minimal build-up on forms — providing longer form lifeRust protect..
Saybolt Viscosity at 210°F 34 SUS
34 SUS
ChevronTexaco Inhibited Transformer Oil
Texaco Transformer Oil and Texaco Transformer Oil Inhibited deliver value through:Prolonged transformer life — Excellent conductive heat transfer properties improve cooling of transformer component..
Saybolt Viscosity at 210°F 34 SUS
34 SUS
ChevronTexaco Transformer Oil
Texaco Transformer Oil and Texaco Transformer Oil Inhibited deliver value through:Prolonged transformer life — Excellent conductive heat transfer properties improve cooling of transformer component..
Saybolt Viscosity at 210°F 34 SUS
34 SUS
ConocoPhillips Transformer Oil
Description: Conoco Transformer Oil, an insulating oil of very high dielectric strength, is suited for oil-filled transformers in both large substations and small pole-mounted transformers. It is al..