Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 152 SUS | 152 SUS | |
ChevronTexaco ISO 460 AIO FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring .. |
|||
Saybolt Viscosity at 210°F | 152 SUS | 152 SUS | ASTM D445 |
ChevronTexaco Regal® 460 Texaco Regal oil delivers value through:Long lubricant life provided by good natural thermal and oxidation stability.Good demulsibility, which assures good lubricant, film strength and reduced wear .. |
|||
Saybolt Viscosity at 210°F | 152 SUS | 152 SUS | ASTM D445 |
ChevronTexaco Regal® 460 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
Saybolt Viscosity at 210°F | 152 SUS | 152 SUS | |
ChevronTexaco Cygnus® 460 Gear Oil Texaco Cygnus Gear Oils deliver value through:High quality control — Enables customer to use lubricants almost as pure as the food being processedHigh performance — Provides lubrication better tha.. |