Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 142 SUS | 142 SUS | |
ConocoPhillips Syncon® 220 Synthetic EP Gear Oil, AGMA No. 5EP Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element .. |
|||
Saybolt Viscosity at 210°F | 142 SUS | 142 SUS | |
ConocoPhillips Hydroclear® 460 Rolling Oil Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi.. |