Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 140 SUS | 140 SUS | |
ChevronTexaco 460 PMO Premium Texaco PMO Premium oils deliver value through:Minimized unscheduled downtime — High oxidation stability provides excellent resistance to deposit formation. The detergent/dispersant additive system .. |
|||
Saybolt Viscosity at 210°F | 140 SUS | 140 SUS | |
ChevronTexaco ISO 460 Industrial Oil EP FeaturesChevron Industrial Oils EP are multipurpose oils for industrial service.Chevron Industrial Oils EP are designed to help minimize wear in all types of plant lubrication and also provide long .. |