Polymer Property : Saybolt Viscosity at 210°F = 117 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 117 SUS
117 SUS
ChevronTexaco 320 Honor Ashless AW
Texaco Honor Ashless AW are circulating oils formulated from high quality base stocks and a carefully balanced, zinc-free additive package. These proved excellent protection against wear for long be..
Saybolt Viscosity at 210°F 117 SUS
117 SUS
ChevronTexaco 320 PMO ashless
Texaco PMO Ashless oils deliver value through:High temperature stability — Contain an effective oxidation inhibitor to protect the oil at elevated ambient operating temperatures.Long lubricant life..
Saybolt Viscosity at 210°F 117 SUS
117 SUS
ChevronTexaco Aries® 320
Texaco Aries lubricants deliver value through:Long equipment life — Extreme pressure performance withstands heavy shock loads typical of rock drill service, protecting the equipment against rapid w..
Saybolt Viscosity at 210°F 117 SUS
117 SUS
ChevronTexaco ISO 320 Machine Oil AW
FeaturesChevron Machine Oils AW are premium quality lubricants.They provide excellent antiwear protection, oxidation and corrosion inhibition, and foam and aeration suppression.They are excellent mu..
Saybolt Viscosity at 210°F 117 SUS
117 SUS
ChevronTexaco Vistac® ISO 320 Rock Drill Oil
FeaturesChevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.They are formulated from highly refined, high viscosity index, paraffinic base stocks and add..
Saybolt Viscosity at 210°F 117 SUS
117 SUS
ChevronTexaco Clarity® ISO 320 Paper Machine Oil
FeaturesChevron Clarity Paper Machine Oils are the next generation circulating oils for the pulp and paper industry.Chevron Clarity Paper Machine Oils ISO 100, 150, and 220 are formulated with ISOS..