Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 107 SUS | 107 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® 6220 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Saybolt Viscosity at 210°F | 107 SUS | 107 SUS | |
ChevronTexaco SAE 75W-90 Manual Transaxle Fluid GL-4 FeaturesChevron Manual Transaxle Fluid GL-4 is a multipurpose lubricant.Chevron Manual Transaxle Fluid GL-4 is formulated with ISOSYN® base stocks and synthetic polymer to meet the severe demands o.. |