Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 996 SUS | 996 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® 6220 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Saybolt Viscosity at 100°F | 996 SUS | 996 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® HTC Chain & Way Fluid, Synthetic Food Grade ISO 220 Description: ANDEROL HTC Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA where incidental fo.. |