Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 92 SUS
92 SUS
ChevronTexaco L Metal Protective Oil L
Texaco Metal Protective Oil L delivers value through:Excellent short-term rust protection — After evaporation of the solvent, a highly protective, nondrying oil film remains which provides a higher..