Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 91 SUS | 91 SUS | |
ConocoPhillips Hydroclear® 15 Rolling Oil Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi.. |