Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 834 SUS | 834 SUS | |
ConocoPhillips SynXPA® 150 R&O Oil Description: Conoco SynXPA R&O Oil lubricates stationary and portable rotary compressors, as well as reciprocating compressors that operate in severe service. It is useful in single- and double-acti.. |