Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 782 SUS
782 SUS
ConocoPhillips 150 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..