Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 7699 SUS | 7699 SUS | |
ChevronTexaco Gear Compounds EP, ISO 1000 Chevron Gear Compounds EP are multipurpose gear lubricants. They provide good thermal stability, extreme pressure protection, antiwear and demulsibility, oxidation, rust, corrosion control and foam .. |
|||
Saybolt Viscosity at 100°F | 7699 SUS | 7699 SUS | |
ChevronTexaco Meropa® 1500 Texaco Meropa oils deliver value through:Gear set efficiencies — High thermal stability EP system maintains clean gear and bearing surfaces, minimizing deposits which interfere with effective lubri.. |