Polymer Property : Saybolt Viscosity at 100°F = 75 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 75 SUS
75 SUS
ChevronTexaco 5606G Aircraft Hydraulic Oil
Texaco Aircraft Hydraulic Oil 5606G delivers value through:Minimum viscosity change over a range of operating temperaturesLow pour point which permits operation at the lowest temperatures generally ..
Saybolt Viscosity at 100°F 75 SUS
75 SUS
ChevronTexaco Superla® 7 White Oil
FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch..
Saybolt Viscosity at 100°F 75 SUS
75 SUS
ChevronTexaco Aviation G Hydraulic Fluid
FeaturesChevron Aviation Hydraulic Fluids are both manufactured from specially selected, highly refined, low viscosity and low pour point petroleum base stocks. They both contain a superior, shear ..