Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Saybolt Viscosity at 100°F = 737 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 737 SUS
737 SUS
ChevronTexaco HiPerSYN™ ISO 150 Oil
FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation stability, high viscosity index, high flash point, low pour point, and e..
Saybolt Viscosity at 100°F 737 SUS
737 SUS
ASTM D-2161
ConocoPhillips ANDEROL® FGC 150 Compressor Fluid, Synthetic Food Grade ISO 150
Description: ANDEROL FGC 150 Compressor Fluid is a synthetic hydrocarbon (PAO) based lubricant formulated with special additive packages that provide good thermal and oxidative stability to keep val..
Copyright © lookpolymers.com All Rights Reserved