Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 677 SUS | 677 SUS | See Note 3. |
ChevronTexaco PremiumRB Texaco Premium RB delivers value through:Wide application range — Suitable for high rpm operation, operating temperatures ranging from -34°C to 177°C (-30°F to 350°F) and offers excellent rust .. |