Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 649 SUS
649 SUS
See Note 3.
ChevronTexaco Thread Compound
Texaco Thread Compound delivers value through:Ability to meet API requirements for high-pressure thread compounds.Galling prevention — Prevents galling in threaded connections. Joints are easier to..