Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 533 SUS
533 SUS
Base Oil Property
ConocoPhillips Moly Poly Grease NLGI No. 2
Description: Conoco Moly Poly Grease is a long-life, lithium 12-hydroxy grease for chassis, wheel bearings, ball joints, U-joints, tie-rod ends, steering knuckles and brake self-adjusting screws fou..