Polymer Property : Saybolt Viscosity at 100°F = 4984.4 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 4984.4 SUS
4984.4 SUS
ChevronTexaco Pinnacle® EP 1000
Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe..