Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 474 SUS
474 SUS
ConocoPhillips Hydroclear® El Mar® 30 Ashless Supreme
Description: Conoco Hydroclear El Mar Ashless Supreme is a premium ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Supreme is speci..