Polymer Property : Saybolt Viscosity at 100°F = 468 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 468 SUS
468 SUS
ASTM D-2161
ConocoPhillips ANDEROL® FGC 40 Compressor Fluid, Synthetic Food Grade ISO 100
Description: ANDEROL FGC 40 Compressor Fluid is a synthetic hydrocarbon (PAO) based lubricant formulated for use in compressors. FGC 40 Fluid meets the former H-1 approval requirements of the USDA w..