Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 32 SUS | 32 SUS | |
Heatbath/Park Speed Quench #1 Water-Based Quenchant An inhibited "brine" quench supplied in granular form to be dissolved in water. While quenching like brine or caustic, it prevents rusting and does not generate disagreeable fumes. Recommended conc.. |