Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 2964 SUS | 2964 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® PQ AA 250 White Mineral Food Grade Gear Oil, ISO Grade 680, SAE Gear Oil Grade 250 Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear.. |