Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 2400 SUS
2400 SUS
Base Oil Property
ConocoPhillips Syncon® Extra Long Life Grease NLGI No. 00
Description: Conoco Syncon Extra Long Life Grease is an ultra high performance lithium-complex grease with heavy synthetic base oil specifically designed for long service life under heavily loaded c..