Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 219 SUS | 219 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® FGC 20 Synthetic Food Grade Compressor Fluid, ISO 46 Description: ANDEROL FGC Series Compressor Fluids are synthetic hydrocarbon (PAO) based lubricants formulated for use in compressors. FGC Series Fluids meet the former H-1 approval requirements of t.. |
|||
Saybolt Viscosity at 100°F | 219 SUS | 219 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® FGH 46 Synthetic Food Grade Hydraulic Fluid, ISO 46 Description: ANDEROL FGH Series Hydraulic Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA wh.. |