Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 212 SUS
212 SUS
ChevronTexaco 46 Heat Transfer Oil
FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont..
Saybolt Viscosity at 100°F 212 SUS
212 SUS
ChevronTexaco Texatherm®
Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging ..