Polymer Property : Saybolt Viscosity at 100°F = 2060 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 2060 SUS
2060 SUS
ChevronTexaco 100 NC Open Gear Lubricant
FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri..