Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 20000 - 30000 SUS
20000 - 30000 SUS
Diluted; ASTM D 445
ConocoPhillips Gear Shield NC Open Gear Lubricant
Description: Conoco Gear Shield NC is a black, viscous fluid designed to lubricate open gears. Gear Shield NC contains neither chlorinated solvents nor lead compounds. Gear Shield NC is designed to ..