Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 182 SUS | 182 SUS | |
ChevronTexaco Transultex® D Texaco Transultex metalworking fluids deliver value through:Excellent antiweld properties from active sulfur and chlorine which reduce frictional heat, prevent welding of metal to the tool point, ex.. |